Plastic Wood Composite Profile Extruding Machine
DESCRIPTION
FEATURES
New revolution Wood Composite Material
Attributes of Wood Composite:
- Recyclabe
- Fire Retardant
- Water Resistant
- Insect Resistant
- Maintenance Free
- High Impact Strength
- No Finishing Required
- Resisitance to Weathering
- Free from Natural Defects
- Close Resemblance to Natural Wood
APPLICATION
- Flooring
- Skirtings
- Wall panels
- Picture frams
- Curtain pole set
- Door and window frams
SPECIFICATION
| Model |
CY-50PW |
CY-65PW |
CY-70PW |
CY-80PW |
CY-100PW |
| EXTRUDING CAPACITY (KGS/HR) |
20 ~ 40 |
30 ~ 55 |
35 ~ 65 |
70 ~ 100 |
70 ~ 100 |
| SCREW DIAMETER (MM) |
50 m/m ø |
65 m/m ø |
70 m/m ø |
80 m/m ø |
100 m/m ø |
PROCESS
PERFORMANCE CHARACTERISTICS
| PROPERTY |
METHOD |
TEST RESULT |
| SPECIFIC DENSITY |
ASTM D648 |
700.00 kg/m³ |
| MOISTURE CONTENT |
ASTM D648 |
1.70% |
| BENDING STRENGTH |
ASTM D1037-93 |
27.74 N/mm² |
| COMPRESSION TEMPERTURE |
ASTM D1037-93 |
11.6749 N/ mm² |
| SOFTENING TEMPERATURE |
ASTM D648 |
83.0℃ |
| FIRE RETARDANT |
UL 94 |
V² |
| SCREW WITHDRAWAL |
BS 6948:1989 |
91.85N |